Gorgar pf NOS BC 
19
The cracking in the surface becomes more obvious now.
19
The cracking in the surface becomes more obvious now.
Viewed: 322 times.

20
The level of the inserts and gaps from wood to plastic are also more obvious.
20
The level of the inserts and gaps from wood to plastic are also more obvious.
Viewed: 293 times.

21
Playfield is  sanded as level as possible at this stage.
21
Playfield is sanded as level as possible at this stage.
Viewed: 300 times.

22
The badly raised inserts are leveling out.They will of course require repaint etc but for this type of playfield it is a better method than removal since it is the inserts themselves that are deformed not there placement in the wood.
22
The badly raised inserts are leveling out.They will of course require repaint etc but for this type of playfield it is a better method than removal since it is the inserts themselves that are deformed not there placement in the wood.
Viewed: 281 times.

23
Same thing other side.
23
Same thing other side.
Viewed: 298 times.

24
Prepped and ready for the next clear.It will take more than just application to work it closer to  level on this pass .The main concern will be trying to seal the gaps in the inserts.
24
Prepped and ready for the next clear.It will take more than just application to work it closer to level on this pass .The main concern will be trying to seal the gaps in the inserts.
Viewed: 283 times.

25
Clear applied.
25
Clear applied.
Viewed: 292 times.

26
26